Powder coating primer containing zinc MT-PZ ALZ55V

MOQ 100KG, From China, B2B only WhatsApp
Brand STD
OEM OEM Services Provided
Advantage Professional, Fast Delivery, Customizable
Samples Apply for free,Contact Export Director now ↓

Surface Finish Options Overview

製品説明

MT-PZ is a powder coating primer containing zinc which is designed to give enhanced corrosion protection of blasted mild steel. This duplex system combines cathodic protection and barrier effect. Dedicated to steel protection with a surface pre-treatment obtained by grit/shot, MT-PZ is based on a specific epoxy zinc rich formulation that promotes conductivity to enhance its cathodic protection. MT-PZ includes a specific anticorrosive function which improves protection even in cases of scratching.

粉末特性

ケミカルタイプThermosetting epoxy
外観スムーズ
色圏グレー
Recommended Film Thickness (µm)70 - 120μm
密度(グラム/ cm3)2.9 ± 0.03 g/cm³
Application静電気
StorageUnder dry, cool (≤ 30°C) conditions
賞味期限At least 12 months from production date

前処理

Surface preparation depends upon the metal, the type of surface, its conditions and the required performance. See our recommendation for pretreatment to be used with MT-PZ.

基板Mechanical pretreatmentChemical pretreatment
軟鋼Grit Blasting Sa 2.5 in accordance with ISO NF EN 8501-1. Roughness: Rz 35 60 µm / Ra 6-12 µm禁止された
鋳鋼
Electro Zinc steel禁止された
溶融亜鉛めっき鋼板
Zinc sprayed (gas flame/electrical deposition)

Application

MT-PZ is suitable for corona electrostatic spraying. Tribo application is not recommended.

アプリケーションの設定Fluidizing air pressure: 1.5kg/cm2 initially then 1kg/cm2

Transport air pressure: 0.5 to 0.8 kg/cm

Recommended voltage: 65 to 70kV

Curing limitsPrimer should be cured, or at least gelled, using the recommended curing schedules, before application of the topcoat. The object temperature must not be below 110°C or above 180°C.

The primer should be cured in a convection oven, optionally with infra-red heaters, with air temperature not exceeding 180°C.

推奨フィルム厚70-120 µm A good protection is linked with the recommended film thickness.
リサイクルTrials, with suitable recycling equipment, must be carried out before commencing production. Attention should be paid to the ratio of new powder, a minimum of 70% must be used. Gun nozzles must be cleaned every 30 minutes.

 

Ready to Start?

For help with solutions customized to your business needs, contact Export Director now.

WhatsApp

Moocy

Export Director

English Russian Español

With 20+ years of experience and We firmly believe that product quality is the basis of cooperation.

Send Inquiry
Online Customer Service
contact

TEl

+86-21-6420 0566

WhatsApp
Service