Main Features of Radiator Powder Coating
Excellent leveling properties, with high gloss and high color saturation
Exceptional adhesion
Good delayed impact resistance; the coating remains highly flexible even after several years
Capable of meeting post-forming requirements and withstanding repeated bending
Superior oil resistance and cooking oil resistance, allowing for repeated cleaning
Energy Efficiency of Radiator Powder Coating
Low-temperature curing (120°C for 25 minutes), saving 25% of baking energy and reducing coating costs.
High transfer efficiency and large coverage area; each kilogram of powder can cover 8-9 square meters, saving 30% of raw materials.
Quality Indicators
Item | Quality Indicator | Test Method |
---|---|---|
Appearance | Uniform color, loose without lumps, dry powder flowability 120-140 mm | Visual inspection |
Color | As per customer requirements | Combination of colorimeter and visual inspection |
Adhesion | Cross-cut test (ISO 2409. GB/T 9286-1998) | 0 level, excellent |
Impact Resistance | Impact tester (drop weight method) (ISO 6272. GB/T 1732-1993) | Good performance at 50 kg.cm |
Bending | Bending test instrument (ISO 1519. GB 6742-1986) | 3 mm, excellent flexibility |
Cupping Test | ISO 1520. GB/T 9753-1993 | Pass at 8 mm |
Surface Hardness | Pencil hardness (Mitsubishi pencil) (ASTM D3363. GB/T 6739-1996) | 1H-2H |
Salt Spray Test | ISO 7253. GB/T 1771-1991 | Over 1000 hours |
Application Fields
Radiators
Other metal workpieces with high heat absorption