Produk Inleiding:
This product is formulated using phenolic epoxy resin and incorporates self-developed conductive polymers and conductive materials, combining the advantages of intrinsic and doped conductivity. It is specifically designed for conductive heavy-duty anti-corrosion powder coatings. The surface resistivity of the coating can reach below 10⁵ Ω, effectively eliminating static electricity accumulation in gas drainage pipes and preventing static sparks, thereby enhancing safety. The coating features high reactivity, strong adhesion, high cross-link density, and excellent resistance to chemicals, solvents, cathodic disbondment, as well as superior flexibility and impact resistance.
Product Features:
Uitstekende adhesie aan die substraat.
Utilizes self-developed materials combining intrinsic and doped conductivity.
Good electrical conductivity of the coating, with surface resistivity reaching 10⁵ Ω, effectively eliminating surface charge accumulation.
Forms an anti-electric field at the coating-metal interface, shielding electron transfer and protecting the metal.
Uitstekende weerstand teen hoë temperatuur katodiese ontbinding.
Lae smelttemperatuur, hoë reaktiwiteit, hoë uithardingsvoltooiingstempo en goeie meganiese eienskappe.
Contains flame retardants, providing certain flame-retardant effects.
Poeierbedekkingsprestasieparameters
| item | Kwaliteit aanwyser | toets Metode |
|---|---|---|
| voorkoms | Eenvormige kleur, geen klonte nie | Visuele inspeksie |
| Digtheid (g / cm³) | 1.3-1.7 | GB / T 4472 |
| Nie-vlugtige inhoud (%) | ≥ 99.4 | GB / T 6554 |
Geharde poeierbedekkingsprestasieparameters
| Toetsitem | Tegniese aanwyser | toets Metode |
|---|---|---|
| voorkoms | Smooth surface, uniform color, no bubbles, cracks, or pinholes | Visuele inspeksie |
| Adhesie (Graad) | 1-3 | CJ / T 120-2008 |
| Impak Weerstand | Geen afskilfering, geen krake nie | CJ / T 120-2008 |
| Surface Resistivity (Ω·m) | ≤ 1×10⁶ (Ω·m) | GB / T 16906-97 |
| Skuurweerstand (1000g, 1000 siklusse) | ≤ 20 g | GB / T 1768-1979 |
| Alcohol Burner Flame Test | Average flaming combustion time ≤ 3s | MT 181-88 |
| Maximum flaming combustion time ≤ 10s | ||
| Average non-flaming combustion time ≤ 20s | ||
| Maximum non-flaming combustion time ≤ 60s | ||
| Buig toets | No stripping or cracking of the inner coating | CJ / T 120-2008 |
| Platmaaktoets (Platmaakverhouding 4/5) | No cracking, no stripping | CJ / T 120-2008 |
Voldoeningstandaard: MT 181-88
Aansoek Fields:
Spesiale antistatiese en anti-korrosie-bedekking vir gasventilasie en dreineringspype in steenkoolmyne.
Aansoekprosesse:
Electrostatic spraying, dip coating, roll coating, etc.
Voorsorgmaatreëls:
The steel pipe surface should be free of oil and moisture; the surface treatment quality should reach Sa2 1/2 level (GB/T 8923); the anchor pattern depth should be 40-90 mm; dust and abrasives on the steel pipe surface should be blown clean. Preheating temperature should be controlled between 180-250°C and must not exceed 275°C.
Die produk moet in 'n goed geventileerde, droë binnenshuise omgewing met 'n temperatuur onder 30°C gestoor word, weg van hittebronne, korrosiewe chemikalieë en chemiese oplosmiddels, en beskerm word teen sterk ligblootstelling. Die stapelhoogte moet nie vier lae oorskry nie. Vermy langtermyndruk en maak seker dat die verpakkingsboks verseël is om koekvorming en vog te voorkom, wat die fluidiseringsprestasie kan beïnvloed.
Om deeglike uitharding van die epoksielaag en beter korrosiewerende werkverrigting te verseker, word dit aanbeveel om die staalpypoppervlak voor te verhit tot bo 200°C om die voltooiing van die uitharding te verbeter.
For help with solutions customized to your business needs, contact Export Director now.
Export Director
With 20+ years of experience and We firmly believe that product quality is the basis of cooperation.
Send InquiryTEl
+86-21-6420 0566