The visual effect achieved from the final headlamp reflector is of the utmost importance and a quality powder primer is the key. The powder coating covers defects in the fabricated part and provides a smooth, corrosion resistant and high reflection finish for the vacuum metallization process. MT-A1270 is an epoxy coating for the application to headlamp reflector casing to provide corrosion protection with a high degree of smoothness in a thin film, prior to the process of metallization under vacuum.
| Химически тип | епоксидна |
| Area of usage | Automotive headlamp reflectors |
| Particle Size Distributon | D50 = 26 – 32 µm Sympatec laser D50 = 30 – 36 µm Malvern laser |
| Външен вид | Extremely smooth, high gloss |
| Цвят | Clear-brown |
| Гланц (60°) | 100 – 120 GU |
| Плътност (g / cm3) | 1.10 0.10 ± |
| Време за желиране при 200°C | 80 – 95 сек. |
| Условия след втвърдяване | 240°C object temperature, 30 minutes holding time (Variations due to oven conditions can be possible but it must be assured by the applicator that it works in his system) |
| Приложение | Електростатичен |
| Стабилност при съхранение | under dry, cool (<23°C) conditions, at least 6 months from production date |
The results are based on mechanical and chemical tests which (unless otherwise indicated) have been carried out under laboratory conditions and are given for guidance only. Actual product performance will depend upon the circumstances under which the product is used.
| Основа | Steel panels |
| Предварителна обработка | Bonder (WH/60/OC) iron phosphate |
| Дебелина на филма | 40 - 60 XNUMX µm |
| График на лечение | 30 minutes 240°C, post cure |
| адхезия | ISO 2409 | GT 0 |
| Твърдост | ISO 2818 | ≥ 125 |
Steel surfaces to be coated must be clean and free from grease. For maximum protection it is essential to pre-treat components prior to the application of MT-A1270. Iron Phosphate and Zinc Phosphate of ferrous metals improve corrosion resistance.
MT-A1270 powders can be applied by manual or automatic electrostatic spray equipment. It is recommended that for consistent application and appearance product be fluidized during application.
For help with solutions customized to your business needs, contact Export Director now.
Export Director
With 20+ years of experience and We firmly believe that product quality is the basis of cooperation.
Send InquiryTEl
+86-21-6420 0566